產(chǎn)品參數(shù)
性能項(xiàng)目 | 試驗(yàn)條件[狀態(tài)] | 測(cè)試方法 | 測(cè)試數(shù)據(jù) | 數(shù)據(jù)單位 | |
物理性能 |
比重
|
ASTM D792 | 1.16 |
g/cm3;
|
|
收縮率 - 流動(dòng) | 3.18 mm | ASTM D955 |
1.5 到 2.5
|
% | |
硬度計(jì)硬度 | 邵氏 A, 10 秒 | ASTM D2240 | 50 | ||
機(jī)械性能 |
剝離強(qiáng)度
|
PP | ISO 813 |
> 6.1
|
kN/m
|
PP (30% VLF) | ISO 813 |
> 6.1
|
kN/m
|
||
PP (50% VLF) | ISO 813 | 3.2 |
kN/m
|
||
拉伸應(yīng)力
|
50%應(yīng)變
|
ASTM D412 | 0.827 |
MPa
|
|
應(yīng)變
|
ASTM D412 | 1.17 |
MPa
|
||
300%應(yīng)變
|
ASTM D412 | 2.96 |
MPa
|
||
抗張強(qiáng)度 | 屈服 | ASTM D412 | 5.52 |
MPa
|
|
伸長(zhǎng)率 | 屈服 | ASTM D412 | 1000 | % | |
撕裂強(qiáng)度 | ASTM D624 | 24.5 |
kN/m
|
||
壓縮變形 |
23℃, 22.0 hr
|
ASTM D395B | 14 | % | |
70℃, 22.0 hr
|
ASTM D395B | 38 | % | ||
可燃性 | UL 阻燃等級(jí) | 1.50 mm, Values per RTP Company testing. | UL 94 |
HB
|
|